ASTM D2000
American Society for Testing and Materials (ASTM) D-2000 Line call-outs ASTM D2000-90
M 2
HK _
7 14
A1-10, B38, C12, EF31, E088, F15,
Z_
DEVIATIONS FROM STANDARD TEST PROCEDURES ADDITIONAL REQUIREMENT SUFFIXES TENSILE STRENGTH (MPa if M IS PRESENT) HARDNESS (DUROMETER)
CLASS
TYPE
GRADE NUMBER
UNITS OF MEASURE
Units of measure: If present an “M” denotes that metric units of measure should be used, i.e. MPa for tensile strength, °C for temperature and kN/m for tear strength.
Grade number 1 = Basic Requirements 2 to 6 = Different requirements as detailed in table 6 of ASTM D2000 this specifies minimum basic requirements for tensile strength, elongation, heat aging, oil immersion and compression set by Classification (Type-class). Appropriate additional requirements apply to each classification, with the grade determining the allowable results.
The values in this guide have been extracted, with permission, from ASTM D2000-12 Standard Classification System for Rubber Products in Automotive Applications. Users should reference and confirm results with the originally published version of ASTM D2000-12. The complete standard may be obtained from ASTM, www.astm.org.